Our company introduced the world's most advanced two Danish Disha casting production lines. Can provide all the spare parts of boiler grate. Customize various sizes according to client’s demand.
Material: HT200, HT250, RTSi5, RQTSi5, RTCr16, RTCr, RTCr2, RTCr5, RTCr2Si4Mo Customize various material according to client’s demand. The product meets the technical standard NB/T 47050-2016.
▌Different Kinds of material for boiler grates
Material |
Advantage |
Shortcoming |
Heat Resistant |
Fuel |
Boiler grate |
HT200 |
Simple process and low cost |
Poor heat resistance and corrosion resistance |
480℃ |
Suitable for low calorific value coal |
Chain grate |
HT250 |
Good strength, wear resistance, heat resistance |
Complex casting and high cost |
520℃ |
Suitable for low calorific value coal |
All the boiler grates |
RTCr |
High oxidation resistance and volume stability |
Poor toughness |
550℃ |
Suitable for low calorific value coal |
Chain grate |
RTCr2 |
High oxidation resistance and volume stability |
Poor toughness |
600℃ |
Suitable for high calorific value coal, biomass |
Suitable for various chains |
Boiler grates and hot water boilers |
|||||
Reciprocating type grate |
|||||
RTCr5 |
Good oxidation resistance and corrosion resistance |
Poor toughness |
700℃ |
Suitable for high calorific value coal, biomass |
Larger grate |
RTCr16 |
Good oxidation resistance and corrosion resistance |
Poor toughness |
900℃ |
Suitable for various high calorific value coals and biomass |
All the boiler grates |
RTSi5 |
Good heat resistance and improved brittleness |
Mechanical and thermal shock force difference |
700℃ |
Suitable for high calorific value coal and biomass |
All the boiler grates |
RTQSi5 |
Good heat resistance and improved brittleness |
Poor corrosion resistance |
800℃ |
Suitable for high calorific value coal and biomass |
All the boiler grates |
RTCr3Si2 |
High temperature strength and high oxidation resistance |
High brittleness at room temperature |
900℃ |
Suitable for high calorific value coal and biomass |
All the boiler grates |
RTQSi2 |
High strength, wear resistance, no deformation, low cost |
Complex casting process |
1200℃ |
Suitable for various coal and biomass |
All the boiler grates |
ZG40CR24 |
Wear resistance, heat resistance, high temperature resistance, long-term non oxidation |
Extremely high production costs |
1250℃ |
Suitable for various coal and biomass |
All the boiler grates |
ZGCr25Ni |
Wear resistance, heat resistance, high temperature resistance, long-term non oxidation |
Extremely high production costs |
1350℃ |
Suitable for various coal and biomass |
All the boiler grates |
RTCr2Si4Mo |
Wear resistance, heat resistance, high temperature resistance, long-term non oxidation |
Extremely high production costs |
1500℃ |
Suitable for various coal and biomass |
All the boiler grates |